# Mammoth Announces Gold Recoveries Of 87% From Bottle Roll Tests On Coarser-Fraction Material From The Large Carneritos Area On Its Tenoriba Gold-Silver Property, Mexico

Canonical Atlas analysis: https://atlas-staging.minestarters.com/news/mammoth-announces-gold-recoveries-of-87-from-bottle-roll-tests-on-coarser-fracti--f1afccb1-fe69-44b1-bac3-26c4c1ce6bac

Original source: https://money.tmx.com/en/quote/MTH/news/6125087818468589/mammoth-announces-gold-recoveries-of-87-from-bottle-roll-tests-on-coarser-fracti

Publisher: tmx

Original announcement: 2026-02-05T18:30:00.000Z

Analysis by Minestarters Atlas

Atlas analysis published: Unknown date

Atlas analysis updated: Unknown date

- Company: Mammoth Resources Corp.

- Ticker: MTH

- Exchange: TSX

- Region: Chihuahua State, Mexico

- Primary commodity: Gold

- Secondary commodities: Silver

- Document categories: Metallurgy

- Extracted: 2026-08-25 22:58:35 UTC

Narrative sentiment: 0.80 · Bullish

## Minestarters Atlas summary

Mammoth Resources reported 87% gold and 67% silver recoveries from bottle roll tests on coarse-fraction oxidized material at the Tenoriba project. These results are comparable to previous fine-fraction testing and suggest strong potential for low-cost heap leach processing of near-surface material.

Reasoning: The results demonstrate that high gold and silver recoveries are achievable even with a much coarser fraction of material, which is a significant de-risking step for future heap leach processing.

- Positive factor: High gold recovery \(87%\) on coarse material

- Positive factor: Favourable comparison to previous fine-fraction testing

- Positive factor: Low cyanide consumption \(0.2 kg/t\)

- Positive factor: Fast leach kinetics \(majority within 12 hours\)

- Positive factor: QA/QC disclosed with QP sign-off

- Negative factor: Higher end of average CaO consumption \(3.8 kg/t\)

Facts used in scoring: 2

## Classification and evidence

**High Recovery**

Polarity: positive

Definition: Recovery at or above the exceptional band for the commodity and processing route.

Why it applies: Gold recovery of 87% on coarse material is within the exceptional/strong band for oxide leach.

Evidence · text

> gave recoveries of 87% gold and 67% silver

**QA/QC Disclosed**

Polarity: positive

Story-specific tag

Definition: Release includes QA/QC disclosure — certified lab, QP sign-off, or stated methods \(blanks, standards, duplicates\).

Why it applies: Release names a Qualified Person \(Richard Simpson\) and a certified laboratory \(SGS\).

Evidence · text

> All cyanide bottle roll tests were performed at the SGS Laboratory... supervised by... a qualified person.

**Bench Scale Only**

Polarity: negative

Definition: Only preliminary bench tests completed — no locked-cycle or pilot work.

Why it applies: Testing was performed using bottle roll tests, which are screening-level bench tests.

Evidence · text

> results from bottle roll tests performed on a coarser-fraction composite sample

## Extracted facts

Stored fact records: 2. Some facts used in scoring do not have a stored record.

## Metallurgical Results (2)

### bottle roll

[Link to this fact](https://atlas-staging.minestarters.com/news/mammoth-announces-gold-recoveries-of-87-from-bottle-roll-tests-on-coarser-fracti--f1afccb1-fe69-44b1-bac3-26c4c1ce6bac#fact-metallurgical-facts-0)

gold

#### Identity

- Commodity: gold
- Ticker: MTH

#### Test Work

- Program Status: preliminary
- Test Type: bottle roll
- Processing Route: cyanide bottle roll
- Sample: composite oxidized coarser-grained material, minus 10-mesh
- Leach Time: 96 hours

#### Recovery

- Recovery: 87 %
- Recovery Basis: actual\_test
- Head Grade: 0.65
- Head Grade Unit: g/t AuEq

#### Reagents

- Cyanide: 0.2 kg/t
- Lime: 3.8 kg/t

#### Lab

- Laboratory: SGS

#### Review

- Needs Review: No
- Historical: No

#### Dates

- Event date: 2026-02-05T00:00:00.000Z

Reasoning: 87% recovery on coarse material is a strong indicator for heap leach viability.

- Positive factor: High recovery on coarse fraction

- Positive factor: Low cyanide consumption

- Negative factor: High CaO consumption

Evidence · text

> Gold dissolution recovery... from the coarser fraction, minus 10-mesh, bottle roll test of composite oxidized coarser-grained material is 87%

### bottle roll

[Link to this fact](https://atlas-staging.minestarters.com/news/mammoth-announces-gold-recoveries-of-87-from-bottle-roll-tests-on-coarser-fracti--f1afccb1-fe69-44b1-bac3-26c4c1ce6bac#fact-metallurgical-facts-1)

silver

#### Identity

- Commodity: silver
- Ticker: MTH

#### Test Work

- Program Status: preliminary
- Test Type: bottle roll
- Processing Route: cyanide bottle roll
- Sample: composite oxidized coarser-grained material, minus 10-mesh
- Leach Time: 96 hours

#### Recovery

- Recovery: 67 %
- Recovery Basis: actual\_test
- Head Grade: 0.65
- Head Grade Unit: g/t AuEq

#### Reagents

- Cyanide: 0.2 kg/t
- Lime: 3.8 kg/t

#### Lab

- Laboratory: SGS

#### Review

- Needs Review: No
- Historical: No

#### Dates

- Event date: 2026-02-05T00:00:00.000Z

Reasoning: 67% silver recovery on coarse material is consistent with previous fine-fraction results.

- Positive factor: Solid silver recovery on coarse material

Evidence · text

> silver recovery is 67%

## How Atlas produces this analysis

Minestarters Atlas uses automated extraction to summarize mining announcements, identify reported measurements, and classify supporting evidence. Sentiment reflects the extracted narrative and classification rules; it is an interpretation, not a reported measurement. Evidence quotes and context are provided where available. Missing data, low-confidence results, and review flags indicate limitations. Check the original publisher announcement before relying on an interpretation.